Experimental investigation of sagging of a completely voided pressure tube of Indian PHWR under heatup condition

Conference proceedings article


Authors / Editors


Research Areas

No matching items found.


Publication Details

Author list: Nandan G, Sahoo PK, Kumar R, Chatterjee B, Mukhopadhyay D, Lele HG

Publisher: Elsevier

Place: LAUSANNE

Publication year: 2010

Journal: Nuclear Engineering and Design (0029-5493)

Journal acronym: NUCL ENG DES

Volume number: 240

Issue number: 10

Start page: 3504

End page: 3512

Number of pages: 9

ISSN: 0029-5493

Languages: English-Great Britain (EN-GB)


View in Web of Science | View on publisher site | View citing articles in Web of Science


Abstract

Pressure tube (zirconium 2.5 wt.% Nb) serves as a pressure boundary for the coolant that removes nuclear heat generated in the reactor core of Indian Pressurised Heavy Water Reactors (IPHWRs). Under postulated low frequency (<10(-6) per year) accidents like Loss of Coolant Accident (LOCA) along with failure of Emergency Core Cooling System (ECCS) injection, heatup of pressure tube (PT) combined with internal pressure and the weight of the fuel bundle may lead to deformation. The extent and nature of deformation is important from reactor safety point of view. An experimental set-up has been designed and fabricated to simulate sagging (downward deformation) of PT due to its own weight and the weight of fuel bundles for 220 MWe IPHWRs. Experiments are conducted at different heatup rates of voided PTs. It is observed that sagging initiates at a temperature around 450 degrees C. Contact between PT and calandria tube (CT) occurs at around 585-625 degrees C, respectively. Once PT-CT contact takes place, PT temperature either decreases or the temperature rise remains controlled whereas CT temperature keeps on increasing for next 20-30 S. The contact location in all the experiments was near the centre of the tube. Structural integrity of PT is retained (no breach) for all the experiments. The PT temperature rise is found to be arrested after the contact between PT and CT, thus establishing that moderator acts as an efficient heat sink for IPHWRs. (C) 2010 Elsevier B.V. All rights reserved.